Table 3.

Tensile parameters of the fibers retrieved in regions I, II and III of the four silking processes

E (GPa)σu (MPa)ϵu
Region I 7.2±0.4 800±70 60±20 
Region II 9.9±0.4 1000±50 34±2 
Region III 9.2±0.6 880±20 30±3 
E (GPa)σu (MPa)ϵu
Region I 7.2±0.4 800±70 60±20 
Region II 9.9±0.4 1000±50 34±2 
Region III 9.2±0.6 880±20 30±3 

Values are means ± s.d.

E, elastic modulus; σu, tensile strength;ϵ u, strain at breaking.