Table 2.

Differences in mechanical properties between adjacent regions

Region interfaceStrain at 2.0 MPa
Modulus at 2.0 Mpa
Change% ChangeChange% Change
a/b (-) 0.265 14.93 (-) 0.706 10.25 
b/c (-) 0.069 4.57 (+) 1.212 19.61 
c/d (-) 0.068 4.72 (+) 1.270 17.18 
d/e (-) 0.079 5.75 (-) 0.562 6.49 
e/f (-) 0.283 21.87 (+) 3.292 40.64 
f/g (-) 0.006 0.59 (+) 0.946 8.30 
g/h (-) 0.053 5.27 (-) 0.254 2.06 
h/i (-) 0.066 6.93 (-) 0.211 1.75 
Region interfaceStrain at 2.0 MPa
Modulus at 2.0 Mpa
Change% ChangeChange% Change
a/b (-) 0.265 14.93 (-) 0.706 10.25 
b/c (-) 0.069 4.57 (+) 1.212 19.61 
c/d (-) 0.068 4.72 (+) 1.270 17.18 
d/e (-) 0.079 5.75 (-) 0.562 6.49 
e/f (-) 0.283 21.87 (+) 3.292 40.64 
f/g (-) 0.006 0.59 (+) 0.946 8.30 
g/h (-) 0.053 5.27 (-) 0.254 2.06 
h/i (-) 0.066 6.93 (-) 0.211 1.75 

Change represents the difference between means of each region.

Sign values (+/-) describe the direction of change in values from anterior to posterior.

The largest change between adjacent regions occurs between regions e and f, coinciding with scale-row reduction.